- PTFE Encapsulated Seals
- Rubber O-Ring,X-Ring
- Spring Energized Seals/Vari Seal
- Hydraulic Rod&Piston Seals
- Hydraulic Piston Seals
- Hydraulic Rod Seals
- Hydraulic Wiper Seals
- Rotary Seals
- Guiding Elements
- Gasket washers Back-up Ring
- Pneumatic Seals& Pneumatic Seal Kits
- Seal Kits
- High-Temperature&Low Temperature Seals
- Rubber Seals
- Oil Seals
- Engineering Plastics Products
- Customized Products
- Add: 3906,Dxing road,Sanshui,Foshan City,528100,Guangdong,China
- Tel: +86 757 87333601
- Fax: +86 757 87333601
- Email: [email protected]
Hydraulic Rod SealsYour position: Home > Hydraulic Rod Seals



HBY
- Rod buffer seal
- buffer seal HBY
- Product description: buffer seal,buffer seal HBY,HBY
Product introduction
HBY is a buffer ring, due to a special structure, facing the sealing lip of the medium reduce the remaining seal formed between the pressure transmission back to the system.Technical Data:
Pressure: below 50 MPa
Temperature: -35 to +110℃
Speed: 0.5m/s
Media: Hydraulic oils (mineral oil-based)
Material: U cups:PU;Back-up ring:POM/PA
Hardness: 90-95 Shore A
Color:Blue,Purple,Off-Yellow
Size: Standard and non-standard