Welcome: BOSS Sealing Solutions

Rotary Oil Seals

  • TC Oil Seal
  • TC Oil Seal
TC Oil SealTC Oil Seal

TC Oil Seal

  • Double lip
  • Iron Framework
  • AS Oil Seal
  • Product description: Double lip TC rotary shaft oil seal
  • INQUIRY
TC oil seal

TC is a double lip oil seal, consist of a sealing lip and a wiper lip. It is widely used in construction machinery,gearbox,pumps and hydraulic motors,etc.

Technical data:

Material: nitrile rubber NBR + iron shell; fluoro rubber FKM + iron shell;
Pressure: 0.5 bar /cm2
Temperature: NBR: -20 ° C / + 100 ° C; FKM: -20 ° C / + 200 ° C
Speed: NBR≤20 m/s; FKM≤40 m/s
Size: Please request.
PREVIOUS:TA Oil Seal NEXT:PTFE Oil Seal