- PTFE Encapsulated Seals
- Rubber O-Ring,X-Ring
- Spring Energized Seals/Vari Seal
- Hydraulic Rod&Piston Seals
- Hydraulic Piston Seals
- Hydraulic Rod Seals
- Hydraulic Wiper Seals
- Rotary Seals
- Guiding Elements
- Gasket washers Back-up Ring
- Pneumatic Seals& Pneumatic Seal Kits
- Seal Kits
- High-Temperature&Low Temperature Seals
- Rubber Seals
- Oil Seals
- Engineering Plastics Products
- Customized Products
- Add: 3906,Dxing road,Sanshui,Foshan City,528100,Guangdong,China
- Tel: +86 757 87333601
- Fax: +86 757 87333601
- Email: [email protected]
Guiding ElementsYour position: Home > Guiding Elements



GT-H phenolic striping
- Phenolic Resin cloth
- Hard Tape
- High Pressure Resist
- Product description: Phenolic Resin Hard Guide Tape
Product introduction
Applications:
GT-H is hard guide tape, it is widely used in hydraulic cylinders,pneumatic cylinders as rod piston guide elements.
Material:
Phenolic resin fiber.
Black,Green,White,Red etc,different color.
Surface:
Rough Surface;
Smooth Surface.